Model No.︰0-150μm
Brand Name︰crigoo
Country of Origin︰China
Unit Price︰CNY ¥ 600 / kg
Minimum Order︰5 kg
GH3230 is a Ni-Cr-based solution-strengthened deformed superalloy with a temperature range of 700-1050 degrees Celsius. The alloy has very good strength and resistance to cold and heat fatigue, and the structure is stable. The alloy has excellent resistance to heat corrosion and oxidation, and is suitable for making parts such as aero engine barrels.
Payment Terms︰ tt